| Carbon steel | Approximately 45–60 W/(m·K), depending on grade and condition. | Often a lower initial material-cost option. Corrosion, coating, inspection, and replacement costs can increase total ownership cost if the fluid or environment is corrosive. | Check for corrosion, erosion, deposits, and coating damage. Water chemistry and corrosion-control measures may be important. | Request material certificates, corrosion allowance details, coating specifications where applicable, inspection guidance, and documented design limits. | Often considered for compatible, relatively non-corrosive services. Confirm corrosion suitability rather than relying on the material name alone. |
| Austenitic stainless steel (for example, 316L) | Approximately 14–16 W/(m·K). | Usually costs more initially than carbon steel. It may reduce corrosion-related maintenance in suitable service, but chloride exposure can cause localized corrosion and costly repairs. | Inspect for pitting, crevice corrosion, fouling, and deposits. Choose cleaning chemicals and procedures compatible with the alloy. | Request confirmation of the exact grade, certificates, weld and fabrication records, chloride-related guidance, and recommended cleaning limits. | Commonly considered for many process and water services. Suitability depends on chloride concentration, temperature, crevices, and other chemistry. |
| Duplex stainless steel (for example, 2205) | Approximately 15 W/(m·K); values vary with grade and condition. | Typically has a higher initial cost than common austenitic grades. In suitable chloride-bearing service, its corrosion resistance and strength may help reduce repair or replacement costs. | Monitor for deposits and localized corrosion. Welding and heat treatment require qualified procedures to preserve the intended material properties. | Request verified grade certificates, qualified welding procedures, fabrication quality records, and guidance on service chemistry and temperature limits. | May be considered where strength and resistance to certain chloride-related corrosion mechanisms are important. It is not immune to corrosion and is not suitable for every chemistry. |
| Titanium (for example, commercially pure Grade 2) | Approximately 17 W/(m·K). | Often has a substantially higher initial material and fabrication cost. It may be economically attractive in some highly corrosive services if it extends service life, but a project-specific lifecycle analysis is essential. | Check for fouling, erosion, and compatibility with the full process chemistry. Avoid unsuitable materials or practices that could contaminate or damage titanium surfaces. | Request traceable material certificates, qualified fabrication and welding documentation, chemistry-specific compatibility review, and clear repair procedures. | Used in selected corrosive services, including some seawater applications. Performance depends on temperature, velocity, crevice conditions, and the presence of specific contaminants. |